PUAFormulation
Formulated product: composition on the TDS
Industrial chemicals

Polyurethane Laminating Adhesives

Technical and industry grades

HS 3506.91
Product family
Chemicals
Forms
Standard grade
Packaging
200 L drums1,000 L IBC
Request TDS / MSDS

What are polyurethane laminating adhesives?

Polyurethane laminating adhesives bond films, foils and paper into multilayer flexible packaging. Most are two-component (2K) systems: an isocyanate prepolymer and a polyol hardener mixed just before use.

They are supplied as solventless (100 % solids) or solvent-based grades dissolved in ethyl acetate, from general-purpose to high-performance retort grades.

Where are PU laminating adhesives used?

They serve flexible-packaging converters that laminate polypropylene BOPP and CPP, PET, foil and polyethylene sealant films. Solvent-based grades are diluted with urethane-grade ethyl acetate; paper laminates may use water-based adhesives.

How are PU laminating adhesives produced?

Each component is made and tested separately.

  • Polyester or polyether polyols react with excess diisocyanate, such as MDI or TDI, to form an NCO-terminated prepolymer.
  • The hardener is formulated from polyols, chain extenders and adhesion promoters.
  • Solvent-based grades are dissolved in dry ethyl acetate; solventless grades contain no solvent.
  • Each lot is tested for NCO content, OH value, viscosity and solids, and the pair is approved for mixing.

PU laminating adhesive types

The table compares the main types; each is then explained with its typical uses.

Solventless 2KSolvent-based 2KWater-based PU
Solids100 %about 50–75 % as suppliedabout 35–50 %
Dry coat weightabout 1.2–2.5 g/m²about 2–4 g/m²about 2–3 g/m²
PerformanceGeneral to medium-highHighest, incl. retortLight to medium
Best forSnacks, dry foods, coffeeRetort, aggressive fillingsPaper, light snack packs

Solventless 2K

No solvent, low energy and fast machine speeds; the most common choice today.

Typical uses
  • Snack and confectionery packs
  • Coffee and pet-food pouches
  • Dairy and frozen-food packs

Solvent-based 2K

Highest heat and chemical resistance for demanding structures.

Typical uses
  • Retort and boil-in-bag pouches
  • Aggressive and spicy fillings
  • Pharma and technical laminates

Water-based PU

Solvent-free dispersions for lighter-duty laminates.

Typical uses
  • Paper and film laminates
  • Light snack packs
  • Labels

Typical data (general-purpose solventless 2K)

ParameterTypical value
Mix ratio, isocyanate : polyolabout 100 : 50–80 by weight
Application temperatureabout 40–60 °C
Mixed viscosity at applicationabout 1,000–3,000 mPa·s
Pot lifeabout 20–40 min
Dry coat weightabout 1.5–2.0 g/m²
Cure before slittingabout 1–3 days at 25–40 °C

The binding specification is the one in our offer and in the Certificate of Analysis for each lot.

Physical properties

PropertyValue
Isocyanate componentClear to amber viscous liquid
Polyol componentClear to hazy viscous liquid
Densityabout 1.05–1.20 g/cm³
Solvent-based flash pointabout −4 °C (ethyl acetate)
Moisture sensitivityIsocyanate reacts with water

How PU laminating adhesives work

  • NCO groups react with OH groups to form a tough, flexible polyurethane network between the films.
  • Water also reacts with NCO and forms CO₂, so moisture causes bubbles and weak bonds.
  • Aromatic isocyanates can form primary aromatic amines (PAA) if cure is incomplete, so food laminates are tested before release.
  • Isocyanate components are skin and respiratory sensitisers (H317, H334). Solvent-based grades ship as UN 1133, Class 3; solventless components are usually not dangerous goods.

PU laminating adhesive applications

Snacks and dry food

BOPP and metallised BOPP laminates for chips, biscuits and confectionery.

Coffee, pet food and dairy

PET/foil/PE pouches with barrier and good seal strength.

Retort and hot fill

PET/foil/CPP structures for sterilised ready meals and sauces.

Pharma and technical

Sachets, blister lidding, labels and insulation laminates.

Main laminating adhesive supplier countries

PU laminating adhesives come mainly from Germany, Italy, Spain, the United States, Japan, China, India and Turkey.

Laminating adhesives in Turkey

Turkey is one of the largest flexible-packaging producers in Europe and uses local and imported laminating adhesives.

Mercafons supplies solventless, solvent-based and water-based PU laminating adhesives to Turkey and the region in drums and IBCs, with documents for each lot.

Laminating adhesive price

The laminating adhesive price depends on isocyanate and polyol costs, performance class, packaging and freight. Request a quote.

PU laminating adhesive packaging

Components are packed separately, moisture-tight and marked with component, lot and expiry date.

200 L drums – Polyurethane Laminating Adhesives packaging | Mercafons
200 L drumsAbout 200–220 kg lined steel or HDPE drums, isocyanate under dry nitrogen.
1,000 L IBC – Polyurethane Laminating Adhesives packaging | Mercafons
1,000 L IBCAbout 1,000–1,100 kg IBCs for large users.

Shipment

Solvent-based grades ship as UN 1133, Class 3; solventless components normally ship as non-dangerous goods. A 20 ft container holds about 16–20 t. See logistics. HS code: 3506.91.

Storage and safety

Storage

Store tightly closed at about 15–30 °C, dry and away from frost. Reseal part-used isocyanate drums under nitrogen. Shelf life is typically 6–12 months.

Safety

Use local exhaust at the laminator, gloves and goggles. In the EU, users of products with more than 0.1 % free diisocyanate need REACH training.

PU laminating adhesive FAQ

Solventless or solvent-based adhesive?

Solventless suits most food packs at lower cost and energy; solvent-based is chosen for retort and very aggressive contents.

How long must laminates cure before use?

Typically 1–3 days for solventless and 3–7 days for solvent-based, until bond strength and PAA tests pass.

What is PAA and why is it tested?

Primary aromatic amines can form from uncured aromatic isocyanate; EU rules require them to be non-detectable in food.

Why do I see bubbles or tunnels in my laminate?

Common causes are moisture, wrong mix ratio, low coat weight or unbalanced web tension.

Is training needed to use these adhesives?

In the EU, REACH requires training for industrial users of products with more than 0.1 % free diisocyanate.

PU laminating adhesive documents: MSDS, TDS and CoA by type

Each system has its own specification. See technical documents.

Last reviewed: November 2026